Certification: | ISO, ISO9001 |
---|---|
Technique: | Tissue Mat |
Mat Type: | AGM |
Customization: |
---|
Shipping Cost:
Estimated freight per unit. |
about shipping cost and estimated delivery time. |
---|
Payment Method: | |
---|---|
Initial Payment Full Payment |
Currency: | US$ |
---|
Return&refunds: | You can apply for a refund up to 30 days after receipt of the products. |
---|
Suppliers with verified business licenses
AGM separator is one kind of environmental-protection material which is made from micro glass fiber(Diameter of 0.4-3um). It is white, innocuity, tastelessness and specially used in Value Regulated Lead-Acid batteries(VRLA batteries). AGM spacer is an ultra-fine glass fiber spacer, featuring small aperture, large number of holes, good mechanical strength, acid corrosion resistance and oxidation resistance, which can effectively prevent the battery from short-circuit phenomenon, and it is an important component in the production of lead storage batteries.We have four advanced production lines with an annual output of 6000T.
Our AGM separator is endowed with the advantages of quick fluid absorption, good water permeability, large surface area, high porosity, good acid resistance and antioxidance, low electric resistance, etc. We adopt advanced technology to meet the high quality requirement.
All of our products are customized in rolls or pieces.
Item
|
Unit
|
AGM Separator
|
Test standard
|
|
GB/T 28535-2012
|
Thickness
|
mm
|
1.75
|
Tensile strength
|
KN/M
|
≥0.79
|
Resistance
|
Ω.dm2
|
≤0.00050d
|
fiber Acid absorption height
|
mm/5min
|
≥80
|
fiber Acid absorption height
|
mm/24h
|
≥720
|
Weight loss in acid
|
%
|
≤3.0
|
Reduction of potassium permanganate material
|
Ml/g
|
≤5.0
|
iron content
|
%
|
≤0.0050
|
Chlorine content
|
%
|
≤0.0030
|
moisture
|
%
|
≤1.0
|
maximum pore size
|
um
|
≤22
|
acid absorption amount with pressure
|
%
|
≥550
|
Suppliers with verified business licenses